Highly resistant to corrosion and chemical attack Easily formed and soldered, with good electrical conductivity Natural inter-metallic bonding Electrolytic tinplate (0.2, 0.3, 0.4 mm thick), otherwise hot dipped To BS 1449 Part 1 CR4; BS 1872; FE/Z/SN/GD; DIN 1623//1541; BS 2920 Tin plating thickness 6 microns, tin purity 99.987% Sheet size 500mm x 300mm (minimum)
Standards
BS 1449 Part 1 CR4; BS 1872; FE/Z/SN/GD; DIN 1623/1541; BS 2920